CMSX-4 Nickel-Based Single Crystal Superalloy Spherical Powder
Properties
Product Name: CMSX-4 Alloy Powder
Shape: Spherical
Density: ~8.7 g/cm³
Melting Point: ~1320–1370°C
Specifications: Customized processing according to customer needs.
Packaging: Vacuum packaging
Particle size: 0-25,15-53,45-105,50-150um Can be supplied according to customer requirements.
Properties: Good high temperature mechanical properties, oxidation resistance.
Usage: Used in aerospace, shipbuilding, industry and other fields.
Products Usage
1. Turbine Blades: Provides long-term reliability in jet engines.
2. Nozzle Guide Vanes: Operates under high thermal and mechanical stresses.
3. Combustion Chambers: Withstands extreme thermal fatigue.
4. Industrial Gas Turbines: Ensures efficiency and durability.
Our normal packaging is 25kgs/Drum
The packaging can be customized. the shipping term can be by sea, by air, and sample or small quantity can be shipped by DHL, FEDEX, EMS and TNT.
Remark: Chemical composition and size can be optimized by the customers' requirements

Conditions for safe storage, including any incompatibilities
Separated from ammonia, strong hydrogen peroxide solutions and strong acids.
Safety Protection
Precautions for safe handling
Handling in a well ventilated place. Wear suitable protective clothing. Avoid contact with skin and eyes. Avoid formation of dust and aerosols. Use non-sparking tools. Prevent fire caused by electrostatic discharge steam.